CP105079 冲击后压缩 概述
CP105079 冲击后压缩 规格型号
Catalog Number |
- |
CP105079 |
Test Standard |
- |
AITM 1-0010 |
Maximum Load | kN kgf lbf | 150 15,000 33,000 |
Temperature Range | °C °F | -75 to +250 -103 to +482 |
Specimen Thickness (Nominal) | mm in | 1 to 10 0.04 to 0.39 |
Specimen Size (Width × Height) | mm in | 100 × 150 3.94 × 5.9 |
Mechanical Connection
Upper Interface (Note 1) |
- | Requires compression platen minimum diameter 50 mm (2 in) |
Lower Interface (Note 1) |
- | Requires compression platen minimum diameter 150 mm (6 in) |
Dimensions
Effective Length (A) | mm in | 200 8.0 |
Overall Width (B) | mm | 220 |
in | 8.4 |
Material |
- | Stainless steel with hardened end loading plates |
Weight (Approximately) | kg | 15 |
lb | 32 |